Characterization of coatings

The characterization of coatings identifies the composition, thickness and structure of a paint, a varnish or a functional coating and measures the properties it gives the part, such as adhesion, hardness, wettability or resistance to weathering and corrosion.

As part of our materials analysis and testing services, we characterize paints, varnishes, lacquers, metallic coatings and functional coatings on metal, plastic or glass. We combine infrared spectroscopy, X-ray fluorescence, optical and electron microscopy, wettability measurements and adhesion, hardness, abrasion, weathering and corrosion tests to validate a formulation, qualify a supplier or explain a defect.

A coating that meets its data sheet can peel, fade or stop protecting when the substrate, the surface preparation or the application process changes. Measuring its properties on the actual part detects those deviations before they reach the line or the customer.

What is the characterization of coatings?

What is it?

Technician examining the surface of a coated sample under an optical microscope during the characterization of coatings

The characterization of coatings is the set of analyses and tests that determine what a coating is made of, how it has been applied and which properties it gives the surface it protects or decorates. It is used to check that a paint, a varnish or a functional treatment meets its specification, to compare formulations or suppliers on the same basis and to identify an unknown coating, for example when it has to be reproduced or a failure has to be explained.

A coating works as a system made up of the substrate, the surface preparation and one or more layers. Its performance depends on the composition of each layer, the thickness, the cure and the bond with the base material, so the same product can perform differently on steel, aluminum, plastic or glass, or depending on how the surface was cleaned before application. That is why testing relies on standard methods for paints and varnishes and on the customer’s specification when it sets its own acceptance criteria.

The variables studied depend on the function of the coating: composition of the resin, pigments or metallic elements, thickness and number of layers, defects such as pores, craters or inclusions, wettability and surface energy, adhesion to the substrate, hardness and resistance to scratching and abrasion, and behavior under ultraviolet radiation, humidity and corrosive environments. The combination of techniques is chosen according to the decision that has to be made.

Paint and coating characterization at INFINITIA

We define the analysis plan from the function of the coating and the question that needs an answer: confirming that a paint meets its specification, choosing between two formulations or explaining why a layer is peeling. With that information we select the techniques, set the acceptance criterion and decide which reference samples are needed.

When the coating is unknown, we identify it before testing it. This was the approach in the coating analysis to resolve adhesion failures in production, where the surfaces were characterized and the compounds present in the layers of some new components were identified to understand their effect on the bond.

If the problem is visual, we use microscopy to compare sound and defective areas. That is the approach of the paint defect analysis using electron microscopy, where the coating surface was observed at different magnifications to locate irregularities and discontinuities that a conventional inspection could not explain.

We deliver a technical report with the techniques and conditions applied, the results for each sample against its reference, images of the defects and the conclusion against the acceptance criterion. If the coating fails, the report shows whether the root cause lies in the formulation, the surface preparation or the application.

Benefits of coating analysis to validate formulations and suppliers

Benefits

The main benefit is confirming with data, on the actual part, that the coating performs the function it was chosen for. Measuring composition, thickness, adhesion and resistance on production samples detects deviations in formulation, preparation or application before they turn into peeling, corrosion or cosmetic rejects.

It makes it possible to compare formulations and suppliers on the same basis. In the evaluation of two steel coatings through electrochemical corrosion testing, the initial characterization of the specimens and the tests on comparable samples provided quantitative data to compare the two solutions.

It shortens the search for the cause of a defect. Identifying the composition and structure of the layers distinguishes between a formulation problem, surface contamination or an incomplete cure, and points the correction to the step in the process where the problem starts, instead of switching products without knowing the cause.

It reduces complaints and the cost of poor quality. Knowing how adhesion, color or gloss evolve after weathering makes it possible to set realistic specifications, accept or reject batches with clear criteria and keep a latent defect, such as weak adhesion, from appearing once the part is already in the customer’s hands.

Technician making a cross-cut through a painted test panel to assess adhesion during the characterization of coatings

Tests and techniques to characterize a coating

Types

Each technique answers a different question about the coating: what it is made of, how it has been applied, how it interacts with liquids and adhesives, how well it withstands use and how it ages. Most studies combine several of them on the same samples.

The sequence matters: first the appearance is documented and the non-destructive techniques are applied, and then those that require cutting or consuming the sample. When samples are compared with a reference, all of them are tested under the same conditions and with the same preparation.

Coating identification and composition

Identification determines what each component of the coating is made of. Infrared spectroscopy (FT-IR) recognizes the resin in paints, varnishes and lacquers, such as epoxy, polyurethane, acrylic or polyester, and some additives; X-ray fluorescence (XRF) and EDX microanalysis identify the elements in metallic coatings, pigments and fillers. The table summarizes what each technique provides.

TechniqueWhat it determinesCoatingDamages sample
FT-IRResin and additivesOrganicMinimal
XRFElementsMetallicNo
SEM-EDXElements by areaAnyDepends on size
Cross-sectionLayers and thicknessAnyYes

Composition makes it possible to confirm that a batch matches the approved formulation, detect a change the supplier did not report or reproduce a coating that has no data sheet. It also explains incompatibilities with adhesives, sealants or topcoats, which depend on the surface chemistry and are not always stated on the data sheet.

Thickness, layer structure and defects

Thickness and structure are studied in cross-section: the sample is cut, mounted and polished to observe each layer under an optical or electron microscope and measure its thickness, its continuity and its bond with the substrate. Examining the surface locates defects such as pores, craters, bubbles, inclusions or cracks that are not visible to the naked eye.

Thickness governs corrosion protection, wear resistance and appearance, and a value out of tolerance reduces protection or promotes cracking. Comparing sound and defective areas of the same part shows whether the defect originates in the application, the cure or prior contamination of the surface.

Wettability, surface energy and roughness

Wettability describes how a liquid spreads over a surface and is quantified by the contact angle of a deposited droplet, measured with a goniometer on the part or on a test panel. Surface energy is calculated from the angles obtained with several liquids, and a profilometer measures the roughness and topography of the coating.

These measurements validate hydrophobic, non-stick or easy-clean coatings and explain why a paint, an ink or an adhesive does not wet a treated surface. Low surface energy hinders the adhesion of the next layer, and roughness changes the appearance, the mechanical anchoring of the coating and how easy it is to clean.

Adhesion of the coating to the substrate

Adhesion indicates how well the coating resists separation from the base material or the previous layer. The cross-cut test in the ISO 2409 standard cuts a lattice pattern through to the substrate and classifies the detachment of the film on a six-level scale, while the pull-off test measures the force needed to pull off a dolly bonded to the surface.

Poor adhesion shows up as blistering, flaking or peeling, and its cause may lie in surface cleaning or preparation, an incomplete cure or incompatibility between layers. The adhesion tests extend these methods to peel, shear and adhesive joints, which are assessed with their own criteria.

Hardness and resistance to scratching and abrasion

The hardness of thin layers is measured by Vickers or Knoop microhardness, with small loads that do not penetrate the coating. Scratch resistance is assessed with scratch tests under controlled load, and abrasion resistance with an abrasion tester that subjects the surface to rubbing cycles, dry, wet or with chemicals, after which the material loss or change in appearance is measured.

These tests validate protective varnishes, hard coatings and anti-scratch treatments on plastic, metal or glass, and compare their durability with that of a reference. The method and criteria for each test are described in the abrasion, scratching and easy cleaning tests.

Weathering and corrosion resistance

Accelerated weathering exposes the coating to radiation, temperature and humidity to anticipate in weeks how it will degrade in service. The ISO 16474-2 standard describes the exposure of paints and varnishes to xenon-arc lamps; afterward, changes in color, gloss and adhesion are measured and the surface is checked for cracking, chalking or blistering.

For corrosion protection, the salt spray test in the ISO 9227 standard is combined with electrochemical tests that quantify the resistance of the layer. The exposure protocols are adapted to each coating and application, and the analysis of galvanized, anodized and coated materials covers metallic and conversion coatings in depth.

Industries where coating analysis prevents rejects and complaints

Sectors

Coatings protect and give appearance to car bodies, steel structures, plastic parts, household appliances, machinery and energy installations, and in each case they face a different environment and failure mode.

That is why the characterization plan is defined from the function of the layer, the substrate and the industry specification, rather than always applying the same set of tests.

Characterization of coatings in automotive and mobility: paints, clear coats and corrosion protection

Body paints, chassis coatings and the clear coats on interior and exterior parts withstand gravel, car washes, solar radiation, road salt and temperature changes throughout the life of the vehicle.

  • Adhesion: cross-cut and pull-off tests verify the bond of each layer, including after exposure.
  • Weathering: ultraviolet radiation and humidity reveal loss of gloss, color changes and cracking.
  • Corrosion: salt spray compares the protection of each paint system on steel and aluminum.

Characterizing the paints and clear coats of production parts makes it possible to approve a change of supplier or process against the same criteria used in the original approval.

Characterization of coatings in metallurgy and metal processing: galvanizing, lacquers and powder coatings

Metal processors apply galvanizing, lacquers, powder coatings and conversion treatments to steel and aluminum, and a deviation in pretreatment or curing can result in entire batches of rejected parts.

  • Surface preparation: cleaning and pretreatment determine how well the layer adheres.
  • Thickness: cross-sections confirm the thickness and continuity of each applied layer.
  • Appearance: microscopy locates the craters, pores and inclusions behind cosmetic rejects.

Characterizing accepted and rejected parts with the same techniques shows at which stage of the coating process the defect originates and which line parameter should be adjusted to correct it.

Characterization of coatings in plastics and rubber: hard coats, metallization and surface treatments

Polycarbonate, ABS or polypropylene parts are varnished, painted or metallized to improve their resistance to scratching, chemicals or radiation, and their low surface energy makes it harder for the applied layers to adhere.

  • Surface energy: contact angle shows whether the pretreatment has activated the surface.
  • Scratching and abrasion: hard coats are compared with abrasion cycles and scratch tests.
  • Chemical exposure: cleaners, creams or fuels can soften or stain the layer.

Combining weathering, abrasion and chemical exposure on the same coating shows whether it keeps its performance under the conditions of use of the final product.

Characterization of coatings in home and consumer goods: non-stick coatings, enamels and decorative finishes

Cookware, household appliances, faucets and furniture carry non-stick coatings, enamels, lacquers or decorative finishes that must withstand washing, heat, cleaning products and daily use for years without losing their appearance.

  • Non-stick performance: contact angle and surface energy quantify how the surface repels water and grease.
  • Cleaning: wet abrasion cycles with detergents reproduce repeated washing.
  • Finish: color, gloss and appearance are compared before and after weathering.

Testing the finished product demonstrates the durability of a finish with data before launch and provides technical arguments in response to a complaint from a customer or a distributor.

Characterization of coatings in machinery and construction: protection against wear and weathering

Machinery components, steel structures and building materials combine anti-corrosion coatings, wear-resistant layers and exterior paints exposed for years to rain, solar radiation and air pollution, often with limited access for repainting.

  • Wear: microhardness and abrasion tests compare hard and self-lubricating coatings under the same conditions.
  • Weathering: accelerated weathering anticipates chalking, fading and loss of protection.
  • Reflectance: optical characterization measures how much solar radiation a roof or facade paint reflects.

Self-lubricating coatings against wear are an example of layers whose selection depends on measuring their hardness, adhesion and abrasion resistance on the actual component.

Characterization of coatings in energy: protection of outdoor equipment and installations

Wind turbine structures, solar panel mounts, tanks and substation equipment rely on paint systems that must protect for years in marine, industrial or high-radiation environments, where maintenance is difficult and costly.

  • Multilayer systems: cross-sections confirm the thickness and bond of primer, intermediate coat and topcoat.
  • Corrosion: electrochemical tests quantify the protection each system provides against saline environments.
  • Radiation: xenon-arc weathering assesses the stability of the topcoat.

Characterizing the system before approving it and after exposure makes it possible to choose between alternatives with comparable data and to plan maintenance on technical grounds.

Characterization of coatings as the basis for specifying, qualifying and solving defects

Value

A coating is bought on the strength of a data sheet and approved against a specification, but only the analysis of the actual part confirms that its composition, thickness and properties match what was agreed. That data turns a discussion with a supplier or a customer into an objective comparison against a measurable criterion.

Characterizing a coating before approving it makes it possible to set realistic specifications: the minimum thickness that protects, the acceptable adhesion rating or how much the color may shift after weathering. With that reference, incoming inspection compares each batch with measured values as well as with the supplier’s certificate, and a formulation change is detected before it reaches the production line. In a complaint, those reference values show whether the coating supplied matches the one approved.

We have FT-IR spectroscopy, X-ray fluorescence, optical and scanning electron microscopy, a goniometer to measure contact angle and surface energy, a profilometer, a microhardness tester, an abrasion tester, a potentiostat, a xenon-arc weathering chamber and a salt spray chamber. We combine these techniques on the same samples, so the results are interpreted together, and we adapt standard methods when the geometry of the part, the size of the sample or the application requires it.

If you are about to approve a new coating, switch suppliers or have parts with peeling, stains or premature corrosion, send us sound and defective samples, the coating data sheet, the substrate and the application process, and the specification it must meet. We will define the characterization plan with you and deliver a technical report with the results, the images and the conclusion against your objective.

Engineer using a magnifier to compare an aged painted panel with its reference to interpret the characterization of coatings

Frequently asked questions about characterization of coatings

FAQs

What can coating analysis not prove?

The analysis shows what the coating on the tested samples is like and how it behaves, but on its own it does not guarantee service life in years or the behavior of batches that have not been analyzed. Hours of weathering or salt spray compare systems with each other and with a reference, without translating directly into years of real exposure.

Nor does it cover stresses that were not applied, such as a specific chemical or a particular cleaning cycle. That is why it is worth defining first which decision the study must support, and then choosing the techniques, the number of samples and the acceptance criterion accordingly.

Why does the same coating behave differently on steel, aluminum or plastic?

Because adhesion and durability depend on the interaction with the substrate as much as on the formulation. Each material has a different surface chemistry, roughness and thermal expansion, and requires its own cleaning and pretreatment for the layer to anchor.

A low surface energy plastic may need activation first, and aluminum without the right pretreatment promotes corrosion under the film. That is why a paint approved on one material is not validated for another, and the tests are repeated on the substrate and the preparation that will be used in production.

Where should you start if only one analysis is possible?

It depends on the question. If the coating is failing, a cross-section examined under the microscope gathers a great deal of information in a single analysis, because it shows the number of layers, their thickness, the bond with the substrate and the point where the defect starts.

If the question is whether a batch matches what was approved, the first technique is chemical identification, compared with a reference sample. That result then determines whether adhesion, weathering or corrosion tests are needed, instead of launching a full test program from the outset that may not answer the question.

Should the actual part be tested, or are flat test panels enough?

Standard methods are applied to flat panels prepared under controlled conditions, which make it easier to compare formulations and suppliers on the same basis. Their limitation is that they do not reproduce the edges, corners, uneven thicknesses or hard-to-reach areas of a real part, which also need to be properly protected.

The most useful approach is to combine both: panels to compare systems and set reference values, and production parts to confirm that the application process achieves those values. When the geometry prevents a standard test, we adapt the method and document the adaptation in the report.

Can a coating be identified without knowing its formulation?

Yes, to a large extent. FT-IR spectroscopy identifies the resin family and some additives, and elemental analysis recognizes pigments, fillers and metals; a cross-section also reveals the number of layers and their thickness. The article on the FT-IR spectrometer explains what kinds of substances it can distinguish.

What cannot be obtained directly is the exact proportion of every component or additives present in very small amounts. To reproduce a coating, identification guides the formulation, which is then validated with the same property tests as the original.

How is the thickness of a multilayer coating measured?

The cross-section is the method that gives the thickness of each layer separately: the sample is cut, polished and each layer is measured under the microscope, which also shows its continuity and the bond between layers. It is destructive and represents the area cut, so several sections are taken when the thickness varies.

For metallic coatings, X-ray fluorescence provides information without damaging the part, within the limitations described in the article on the portable XRF gun. The choice depends on whether the total thickness, the thickness of each layer or a quick measurement on many parts is needed.

How can you tell whether a defect starts in the substrate, in the application or later?

From the position of the defect in the cross-section and from what is found in it. If it starts at the interface with the substrate, it points to cleaning, pretreatment or prior corrosion; if it is inside the film, to the application or the cure; if it is only on the surface, to later contamination or damage.

Microanalysis of the affected area confirms the hypothesis, for example by detecting traces of oil, salts or foreign particles under the layer. Comparing it with a sound area of the same part avoids mistaking a defect for a normal feature of the system.

Why does a paint peel after passing the adhesion test?

Because the initial test assesses adhesion at the time of testing and under the conditions of the test panel. Humidity, thermal cycling, radiation or cleaning products can degrade the interface over time, and a production part may arrive with contamination or a pretreatment different from that of the tested sample.

That is why it is worth measuring adhesion after weathering or humidity exposure as well, and doing so on production parts. If the paint fails only in some areas, analyzing those areas against sound ones points toward the cause.

How much does coating characterization cost and what does it depend on?

It depends on the techniques, the number of samples and references, the duration of the weathering or corrosion tests and the subsequent analysis. A chemical identification or a cross-section costs less than a weathering campaign lasting several weeks with adhesion and color measurements at each stage.

To give you a firm quote, tell us which coating and substrate you want to analyze, how many samples you have, which specification or standard you must meet and which decision depends on the result. With that information we will propose the characterization plan best suited to your objective.

How long does it take to get results?

Typical lead times range from 1 to 4 weeks, depending on the techniques, the duration of the tests and the subsequent analysis. A chemical identification, a contact angle measurement or a cross-section can be completed in a few days, while accelerated weathering and salt spray take several weeks of exposure alone.

If you need the result urgently, a 24 to 72 hour option can be considered on a case-by-case basis, when the study does not require long exposures. Tell us the date by which you need the data and send the samples labeled and with the available documentation.

Can you check whether a supplier has changed the coating formulation?

Yes, as long as a reference sample from the approved batch exists. Comparing the FT-IR spectrum, the elemental composition and the thickness of each layer in the suspect batch with those of the reference shows whether the resin, pigments or fillers have changed, even if the appearance is the same.

To make that comparison possible, keep samples from the batch you qualified, along with its data sheet and test report. If you detect a change, the next step is to test the properties that are critical for your application, such as adhesion or corrosion resistance, and decide whether the batch is acceptable.

Which samples should I send and how should I prepare them?

Send parts or panels with the coating you want to analyze and, if you are investigating a defect, sound and defective parts from the same batch or production date, labeled separately. Include the coating data sheet, the substrate, the pretreatment and the application process, and the specification it must meet.

Do not clean the affected area or touch it with bare hands, because you could remove the residues that explain the failure. Protect the surfaces with clean paper, without adhesive tape on the coating, and pack each part separately in a rigid box to prevent rubbing during shipping.

Adhesives - coatings - treatments

Tell us about your case

For a priority response, please contact us using the form below.